DIN 17175 Seamless Tubes of Heat-resistant Steels
Chemical Composition of DIN 17175 10CrMo910 Alloy Steel Pipes
C % | Mn % | P % | S % | Si % | Cr % | Mo % |
0.08-0.15 | 0.40-0.70 | 0.035 max | 0.035 max | 0.50 max | 2.0-2.50 | 0.90-1.20 |
Mechanical Properties of DIN 17175 10CrMo910 Alloy Steel Pipes
Tensile Strength, Mpa | Yield Strength, MPa | Elongation, % |
450-600 min | 280 min | 20 min |